Home\Cases\Aviation & Aerospace\Superalloy Side Milling Semiconductors Aviation & Aerospace Medical Consumer Electronics General Precision Manufacturing Automotive Semiconductors Aviation & Aerospace Medical Consumer Electronics General Precision Manufacturing Automotive Superalloy Side Milling Workpiece Superalloy GH4169 Challenges Short tool life (avg. machining length 60 meters/tool) Benefits Lower cutting force and reduced tool wear with ultrasonic machining Machining length per tool increased by 33% to avg. 80 meters Workpiece Benefits Nomex Honeycomb Contouring图片宽度:400px, 图片高度:293px ChallengesUneven machined surface, severe burrs and excessive dustVulnerable to workpiece deformation, tearing and collapse due to compression Burr reduction by 90%Efficient 5-axis contouring of complicated shapesOptional fully-closed protection and vacuum system against dust and explosion WorkpieceNomex Honeycomb Contouring ChallengesUneven machined surface, severe burrs and excessive dustVulnerable to workpiece deformation, tearing and collapse due to compressionBenefitsBurr reduction by 90%Efficient 5-axis contouring of complicated shapesOptional fully-closed protection and vacuum system against dust and explosion RELATED CASES AlSiC Threaded Hole Machining More Quartz Glass Substrate Chamfer & Side Machining More Quartz Glass Showerhead Drilling More Single Crystal Silicon Showerhead Hole Drilling More Single Crystal Silicon Showerhead Hole Drilling More